C110 Copper (ETP)
Electrolytic Tough Pitch Copper
One of the most widely used copper alloys due to its excellent electrical conductivity, reliable performance, and broad availability. It is commonly used in electrical components, telecommunications infrastructure, and industrial equipment where consistent conductivity and formability are critical. At Comet Metals, we supply C110 copper foil, sheet, and coil materials supported by precision converting services. Our team works closely with manufacturers and engineers to ensure materials meet specification and arrive ready for production.
Material Range
Comet Metals maintains aluminum inventory and converting capabilities across a wide range of sizes and formats.
| Thickness: | .0007” to .100” |
| Widths: | .200” to 36” |
| Tempers: | Ann, 1/4, 1/2, 3/4, full hard and spring |
| Finishes: | Commercial and bright finish |
Built for use by:
Infrastructure
Automotive
Manufacturing
HVAC
Aerospace
Medical
Electronics
Specifications
| Alloy Class | Coppers |
| Alloy Name | ETP Copper |
| CDA Number | 110 |
| ASTM Standards | B-152 |
| Principal Design Features | Extremely soft and easy to work with. Most common copper alloy used. Conductivity 101% IACS. |
| Applications | Primarily an electrical component in transformers, switchgear, and parts requiring high electrical conductivity. Also many design applications. |
| Annealing | Can be annealed between 700 and 1200°F; available in annealed, 1/4, 1/2, 3/4, and full hard tempers. |
| Cold Working | Easily completed. |
| Forging / Hot Working | Can be forged and easily hot worked. |
| Welding | Soldering is superb and it can be brazed in many applications. Welding in environments that must exclude oxygen is not recommended. |
Chemical Properties
| Copper (Cu) | 99.9% (Min.) |
| Oxygen (O2) | 0.05% (Max.) |
| Nickel (Ni) | – |
| Phosphorus (P) | – |
| Tin (Sn) | – |
| Zinc (Zn) | – |
Mechanical Properties
| Elongation (Annealed) | 20 to 50 |
| Elongation (1/4 Hard) | 13 to 33 |
| Elongation (1/2 Hard) | 8 to 32 |
| Elongation (3/4 Hard) | 5 to 24 |
| Elongation (Hard) | 3 to 16 |
| Elongation (Extra Hard) | 3 to 5 |
| Elongation (Spring) | 2 to 4 |
| Elongation (Extra Spring Hard) | 3 (Max) |
| Rockwell (Annealed) | F 75 (Max) |
| Rockwell (1/4 Hard) | 18 to 51 |
| Rockwell (1/2 Hard) | 43 to 47 |
| Rockwell (3/4 Hard) | 47 to 49 |
| Rockwell (Hard) | 54 to 62 |
| Rockwell (Extra Hard) | 56 to 64 |
| Rockwell (Spring) | 60 to 66 |
| Rockwell (Extra Spring) | 61 (Min) |
| Tensile Strength (Annealed) | 26 to 38 |
| Tensile Strength (1/4 Hard) | 34 to 42 |
| Tensile Strength (1/2 Hard) | 37 to 46 |
| Tensile Strength (3/4 Hard) | 41 to 50 |
| Tensile Strength (Hard) | 43 to 52 |
| Tensile Strength (Extra Hard) | 47 to 546 |
| Tensile Strength (Spring) | 50 to 58 |
| Tensile Strength (Extra Spring Hard) | 52 (Min) |
| Yield Strength (Annealed) | 6 to 13 |
| Yield Strength (1/4 Hard) | 26 to 39 |
| Yield Strength (1/2 Hard) | 30 to 44 |
| Yield Strength (3/4 Hard) | 39 to 48 |
| Yield Strength (Hard) | 41 to 50 |
| Yield Strength (Extra Hard) | 46 to 55 |
| Yield Strength (Spring) | 48 to 57 |
| Yield Strength (Extra Spring Hard) | 51 (Min) |
Physical Properties
| Electrical Conductivity | 101% IACS |
| Thermal Conductivity | 226 BTU/sq.ft/hr/°F |
| Density | 0.323 lbs./cu.in. |
| Coefficient of Thermal Expansion | 9.8 in/in/°F x 10^6 (68°F to 572°F) |
| Modulus of Elasticity | 17 x 10^6 psi |
More Copper materials
Oxygen-Free Copper 101, 102 & 103
Oxygen-free grades for work where conductivity and thermal performance cannot be compromised.